How to print TPU and other flexible filaments

Speeds, temperatures, retraction and infill for TPU, plus which printers handle it well and the flexible prints worth making: phone bumpers, feet, grips and seals.

TPU is the rubbery filament behind phone bumpers, non-slip feet, watch straps, gaskets and squishy toys. It is very forgiving once printing, but it hates being pushed fast. Here is how to get it right the first time.

Know your TPU: Shore hardness

Flexible filaments are rated on the Shore A scale. Lower is softer.

Hardness Feels like Ease of printing
98A to 95A Firm rubber, a phone case Easiest, works on most printers
90A to 85A Shoe sole, soft grip Needs a direct-drive extruder
Below 85A Gummy, very stretchy Hard; slow and tuned printers only

If you are new to flexibles, start with 95A.

Direct drive vs. Bowden

On a direct-drive printer (the extruder sits right above the hotend, as on most modern Bambu Lab, Prusa and Creality machines) TPU prints easily. On a Bowden printer the soft filament can buckle in the long tube: it still works with 95A, but very slowly.

Starting settings

  • Nozzle temperature: 220 to 240 °C (follow the spool label)
  • Bed temperature: 40 to 60 °C. TPU sticks very well, so use a glue stick on smooth PEI as a release layer.
  • Speed: 20 to 40 mm/s, with a low volumetric flow (about 3 to 5 mm³/s). This is the single most important setting.
  • Retraction: small or off. Start with 0.5 to 1 mm on direct drive. Big retractions jam flexible filament.
  • Cooling: 50 to 100% fan after the first layers.
  • Travel: enable "avoid crossing perimeters" to limit stringing.

Most slicers ship a "Generic TPU" profile that is a good starting point.

Infill decides how soft the part feels

With TPU, infill is your squishiness knob.

  • 0 to 10% gyroid: soft and bouncy
  • 15 to 30% gyroid: a good general purpose feel
  • Solid: firm, like a hard rubber stopper

Gyroid infill is the usual choice because it flexes evenly in every direction.

Dry it first

TPU absorbs moisture fast. Wet TPU hisses, strings badly and prints rough, foamy walls. Dry it before printing (a filament dryer or about 50 °C for 4 to 6 hours) and print straight from a dry box if you can.

Common problems

  • Filament tangles in the extruder: slow down, reduce retraction, check the filament path for gaps.
  • Heavy stringing: dry the filament, lower the temperature 5 °C, enable "avoid crossing perimeters."
  • Part fused to the bed: use glue stick as a release agent; let the bed cool before removing.

Great things to print in TPU

  • Non-slip feet and bumpers for furniture and gadgets
  • Phone bumpers and cases (print a test fit first)
  • Cable ties and strap loops
  • Grips for tools, pens and bike handlebars
  • Seals and gaskets for jars and project boxes
  • Squishy fidget toys and pet toys

Browse Home & Organization and Workshop for parts that work well in TPU, and see PLA vs PETG for the other everyday filaments.